Spring Flat
Description:Spring flat, Flat spring clip.
Send Email Details
Technical information:
1. Material: Spring steel
2. Surface treatment: None
3. Process: Progressive Stamping --- Degreasing
Engineering difficulty:
1. Structure and shape is complex.
2. All the 12 wings should be parallel on the horizontal vertical direction.
3. No deformation after the wings are flipped over 300 times.
Remarks:
1. Tooling time: 13 working days
2. Production time: 13 working days
3. Usage: Automobile / Heavy Equipment -
Steel Washer
Description: Steel washer, Stainless steel washer.
Send Email Details
Technical information:
1. Material: Stainless steel
2. Surface treatment:None
3. Process: Progressive Stamping --- Degreasing
Engineering difficulty:
Customized dimension, low unit price
Remarks:
1. Tooling time: 10 working days
2. Production time: 12 working days
3. Usage: Air Monitor / toothbrushes -
Spring Steel Clip
Description: Spring steel clip, Flat spring.
Send Email Details
Technical information:
1. Material: Spring steel
2. Surface treatment: Black electrophoresis
3. Process:Progressive Stamping --- Black electrophoresis
Engineering difficulty:
1. Highly adhesive force.
2. Coating can't be get off in abrasion environment.
Remarks:
1. Tooling time: 14 working days
2. Production time: 13 working days
3. Usage: Construction hotels retails / Metal & Metallurgy Machinery Parts